| Processing Techniques | Equipment name & NEMO ID | Teaser Blurb | Cleanliness | Location |
|---|---|---|---|---|
| Step Profile |
Profilometer AlphaStep D-300 alphastep2 |
A stylus-based (tip radius 2 microns) surface profiler that measures step heights from 50nm to 300 µm on materials.
|
Flexible | SNF Exfab Paul G Allen L104 Stinson |
| Step Profile | Dektak XT-S Stylus Profiler SNSF NPC |
Surface profiler measures step heights as small as 10nm. Stylus tip radius is 12.5 microns. |
SNSF NPC Spilker suite 6 | |
| Step Profile |
Profilometer Alphastep 500 alphastep |
Surface profiler measures step heights from 500 Å to 300 µm on materials in the flexible cleanliness group. Scan length from 100 Angstroms up to 0.3 mm. Stylus tip radius is 5 µm.
|
Flexible | SNF Exfab Paul G Allen L104 Stinson |