Processing Techniques Equipment name & NEMO ID Teaser Blurb Cleanliness Locationsort ascending
Step Profile Dektak XT-S Stylus Profiler SNSF NPC

Surface profiler measures step heights as small as 10nm. Stylus tip radius is 12.5 microns.

SNSF NPC Spilker suite 6
Step Profile Profilometer Alphastep 500
alphastep

Surface profiler measures step heights from 500 Å to 300 µm on materials in the flexible cleanliness group. Scan length from 100 Angstroms up to 0.3 mm. Stylus tip radius is 5 µm.

 

Flexible SNF Exfab Paul G Allen L104 Stinson
Step Profile Profilometer AlphaStep D-300
alphastep2

A stylus-based (tip radius 2 microns) surface profiler that measures step heights from 50nm to 300 µm on materials.  

 

Flexible SNF Exfab Paul G Allen L104 Stinson